tobrien, it's first time I'm working with Titanium so I've try deferent methods and still trying
Hydro-abrasive produce smooth edges but pure accuracy with small holes. Argon plasm better in shapes but 'obloy' (burrs) large and extremely hard
All rings filed, sanded and polished (all surfaces exclude inner and clasp holes) but due material hardness there are some roughness (more noticeable than stainless ones) remains
Hydro-abrasive produce smooth edges but pure accuracy with small holes. Argon plasm better in shapes but 'obloy' (burrs) large and extremely hard
All rings filed, sanded and polished (all surfaces exclude inner and clasp holes) but due material hardness there are some roughness (more noticeable than stainless ones) remains